dc.description.abstractEnThe use of a slow cooling ramp is the only way to significantly reduce the presence of typical defects within the welds for this Pd-based alloy studied.
dc.language.isoen
dc.publisherElsevier
dc.title.enEffect of temporal pulse shaping on the reduction of laser weld defects in a Pd-Ag-Sn dental alloy.
dc.typeArticle de revue
dc.identifier.doi10.1016/j.dental.2010.10.012
dc.subject.halChimie/Matériaux
bordeaux.journalDental Materials
bordeaux.pagee43-e50
bordeaux.volume27
bordeaux.issue3
bordeaux.peerReviewedoui
hal.identifierhal-00575875
hal.version1
hal.popularnon
hal.audienceInternationale
hal.origin.linkhttps://hal.archives-ouvertes.fr//hal-00575875v1
bordeaux.COinSctx_ver=Z39.88-2004&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.jtitle=Dental%20Materials&rft.date=2011&rft.volume=27&rft.issue=3&rft.spage=e43-e50&rft.epage=e43-e50&rft.eissn=0109-5641&rft.issn=0109-5641&rft.au=BERTRAND,%20Caroline&POULON-QUINTIN,%20Angeline&rft.genre=article


Files in this item

FilesSizeFormatView

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record