Show simple item record

hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorELISSALDE, Catherine
hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorCHUNG, U-Chan
hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorJOSSE, Michaël
hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorGOGLIO, Graziella
hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorSUCHOMEL, Matthew
hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorMAJIMEL, Jérrôme
hal.structure.identifierCentre interuniversitaire de recherche et d'ingénierie des matériaux [CIRIMAT]
dc.contributor.authorWEIBEL, Alicia
hal.structure.identifierInstitut de Chimie de la Matière Condensée de Bordeaux [ICMCB]
dc.contributor.authorSOUBIE, F.
hal.structure.identifierCentre interuniversitaire de recherche et d'ingénierie des matériaux [CIRIMAT]
dc.contributor.authorFLAUREAU, Andréas
hal.structure.identifierCentre interuniversitaire de recherche et d'ingénierie des matériaux [CIRIMAT]
dc.contributor.authorFREGEAC, Arnaud
hal.structure.identifierCentre interuniversitaire de recherche et d'ingénierie des matériaux [CIRIMAT]
dc.contributor.authorESTOURNES, Claude
dc.date.issued2019-07
dc.identifier.issn1359-6462
dc.description.abstractEnThe densification of zirconia at very low temperatures (<400 °C) requires enhanced synergy between thermodynamics and kinetics. This work demonstrates an efficient single step approach combining amorphous hydrated zirconia and Spark Plasma Sintering at 350 °C and 600 MPa. The resulting zirconia ceramics exhibit a cohesive nanostructure with small average grain sizes (20 nm) and a predominantly monoclinic structural polymorph confirmed by both X-ray scattering analyses and High Resolution Transmission Electronic Microscopy. Remarkable Vickers hardness of 3.8 GPa for high level of porosity (30%) is explained by the density and homogeneous distribution of grains boundaries and meso/microporosities.
dc.language.isoen
dc.publisherElsevier
dc.subject.enAmorphous oxides precursors
dc.subject.enNanostructured zirconia ceramics
dc.subject.enPolymorphic phase transformation
dc.subject.enHardness
dc.subject.enSpark plasma sintering
dc.title.enSingle-step sintering of zirconia ceramics using hydroxide precursors and Spark Plasma Sintering below 400 °C
dc.typeArticle de revue
dc.identifier.doi10.1016/j.scriptamat.2019.04.037
dc.subject.halChimie/Matériaux
bordeaux.journalScripta Materialia
bordeaux.page134-138
bordeaux.volume168
bordeaux.peerReviewedoui
hal.identifierhal-02125329
hal.version1
hal.popularnon
hal.audienceInternationale
hal.origin.linkhttps://hal.archives-ouvertes.fr//hal-02125329v1
bordeaux.COinSctx_ver=Z39.88-2004&amp;rft_val_fmt=info:ofi/fmt:kev:mtx:journal&amp;rft.jtitle=Scripta%20Materialia&amp;rft.date=2019-07&amp;rft.volume=168&amp;rft.spage=134-138&amp;rft.epage=134-138&amp;rft.eissn=1359-6462&amp;rft.issn=1359-6462&amp;rft.au=ELISSALDE,%20Catherine&amp;CHUNG,%20U-Chan&amp;JOSSE,%20Micha%C3%ABl&amp;GOGLIO,%20Graziella&amp;SUCHOMEL,%20Matthew&amp;rft.genre=article


Files in this item

FilesSizeFormatView

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record