Microwave synthesis of lithium lanthanum titanate
Language
en
Article de revue
This item was published in
Solid State Communications. 2003, vol. 125, n° 10, p. 557-562
Elsevier
English Abstract
A microwave method has been developed for the preparation and sintering of lithium lanthanum titanate (LLTO) of the formula Li0.35La0.55TiO3. The method is fast, clean, economical and gives phase pure product of high conductivity.
A microwave method has been developed for the preparation and sintering of lithium lanthanum titanate (LLTO) of the formula Li0.35La0.55TiO3. The method is fast, clean, economical and gives phase pure product of high conductivity.Read less <
English Keywords
Microwave synthesis
Solid electrolytes
Lithium batteries
Origin
Hal imported